USE FORM |
ADVANTAGES
COMPOSITION
Blend of tension-active foaming agents and specific additives.
INSTRUCTIONS FOR USE
And 3 to 7 litres of POLYMOUSSE/ M3 of water.
Pour POLYMOUSSE directly in water.
In unconsolidated formations, first make a drilling mud (1 Kg POLYCOL 60 S or 2 litres POLYCOL 60 LS/ M³ of water) and then add 3 to 7 litres of POLYMOUSSE.
The concentration depends on water inlet in the hole.
Inject 10 to 30 litres of mixture through the drill rods. Then add air while drilling.
In unconsolidated layers, sometimes it is necessary to make an injection every meter. So it is better to inject the mixture through a pump.
POLYMOUSSE is compatible with nearly all kinds of polymers for drilling muds and foaming agents.